GGG -DUCTILE IRON |
|||||
EN 1563 1997-08 |
Rm N/mm² min |
Rp 02 N/mm² min |
A5 % |
HARDNESS HB |
MICRO - STRUCTURE |
EN-GJS-400-15 |
400 |
250 |
15 |
130 - 180 |
Ferrite |
EN-GJS-400-18 LT |
400 |
240 |
18 |
120 - 180 |
Ferrite |
EN-GJS-400-18 RT |
400 |
250 |
18 |
120 - 180 |
Ferrite |
EN-GJS-500-7 |
500 |
320 |
7 |
170 - 220 |
Ferrite / Pearlite |
EN-GJS-600-3 |
600 |
370 |
3 |
200 - 250 |
Pearlite / Ferrite |
| GG - GRAY CAST IRON |
||
EN 1561 1997-08 |
Rm Ø30 N/mm² |
HARDNESS Ø30 HB MAX |
EN-GJL-200 |
200 |
210 |
EN-GJL-250 |
250 |
230 |
EN-GJL-300 |
300 |
270 |